Sandeep Bhattacharya, Ph.D. - Publications

Affiliations: 
2014 ENGINEERING MATERIALS University of Windsor, Windsor, Canada 
Area:
Materials Science Engineering, General Engineering, Alternative Energy

19 high-probability publications. We are testing a new system for linking publications to authors. You can help! If you notice any inaccuracies, please sign in and mark papers as correct or incorrect matches. If you identify any major omissions or other inaccuracies in the publication list, please let us know.

Year Citation  Score
2020 Khattra NS, Bhattacharya S, Lauritzen MV, Kjeang E. Residual fatigue life modeling of fuel cell membranes Journal of Power Sources. 477: 228714. DOI: 10.1016/J.Jpowsour.2020.228714  0.307
2020 Bhattacharya S, Leung J, Lauritzen M, Kjeang E. Isolated chemical degradation induced decay of mechanical membrane properties in fuel cells Electrochimica Acta. 352: 136489. DOI: 10.1016/J.Electacta.2020.136489  0.326
2019 Cui Z, Bhattacharya S, Green DE, Alpas AT. Mechanisms of die wear and wear-induced damage at the trimmed edge of high strength steel sheets Wear. 1635-1645. DOI: 10.1016/J.Wear.2019.01.113  0.576
2018 Bhattacharya S, Alpas AT. A novel elevated temperature pre-treatment for electrochemical capacity enhancement of graphene nanoflake-based anodes Materials For Renewable and Sustainable Energy. 7. DOI: 10.1007/S40243-018-0110-3  0.57
2018 Sun G, Bhattacharya S, White DR, McClory B, Alpas AT. Indentation Fracture Behavior of Low Carbon Steel Thermal Spray Coatings: Role of Dry Sliding-Induced Tribolayer Journal of Thermal Spray Technology. 27: 1602-1614. DOI: 10.1007/S11666-018-0799-7  0.564
2017 Bhattacharya S, Alpas AT. Effects of Electrolyte Composition and Voltage Scan Rate on Cyclic Performance of Silicon-Aluminum Anodes for Lithium-Ion Cells Ecs Transactions. 75: 1-15. DOI: 10.1149/2.1321709Jes  0.598
2017 Sun G, Bhattacharya S, Alpas AT. Cyclic strain-induced crack growth in graphite during electrochemical testing in propylene carbonate-based Li-ion battery electrolytes Journal of Materials Science. 53: 1297-1309. DOI: 10.1007/S10853-017-1547-Y  0.621
2016 Dutta T, Kim KH, Uchimiya M, Kumar P, Das S, Bhattacharya SS, Szulejko J. The micro-environmental impact of volatile organic compound emissions from large-scale assemblies of people in a confined space. Environmental Research. 151: 304-312. PMID 27522568 DOI: 10.1016/J.Envres.2016.08.009  0.39
2016 Das S, Deka P, Goswami L, Sahariah B, Hussain N, Bhattacharya SS. Vermiremediation of toxic jute mill waste employing Metaphire posthuma. Environmental Science and Pollution Research International. PMID 27117148 DOI: 10.1007/s11356-016-6718-x  0.403
2016 Bhattacharya S, Alpas AT. Self-healing of cracks formed in Silicon-Aluminum anodes electrochemically cycled at high lithiation rates Journal of Power Sources. 328: 300-310. DOI: 10.1016/J.Jpowsour.2016.07.118  0.64
2015 Bhattacharya S, Shafiei M, Alpas AT. Microstructural Characterization of Nanocrystalline Sn-Coated Carbon Fibre Electrodes Cycled in Li-Ion Cells Metallurgical and Materials Transactions E. 2: 208-219. DOI: 10.1007/S40553-015-0058-5  0.619
2014 Bhattacharya S, Riahi AR, Alpas AT. Electrochemical cycling behaviour of lithium carbonate (Li 2CO3) pre-treated graphite anodes - SEI formation and graphite damage mechanisms Carbon. 77: 99-112. DOI: 10.1016/J.Carbon.2014.05.011  0.742
2014 Bhattacharya S, Riahi AR, Alpas AT. Thermal cycling induced capacity enhancement of graphite anodes in lithium-ion cells Carbon. 67: 592-606. DOI: 10.1016/J.Carbon.2013.10.032  0.719
2013 Bhattacharya S, Alpas AT. Role of sliding-induced tribofilms on fracture of particles in aluminium-silicon alloys Wear. 301: 707-716. DOI: 10.1016/J.Wear.2013.01.081  0.608
2012 Bhattacharya S, Alpas AT. Micromechanisms of solid electrolyte interphase formation on electrochemically cycled graphite electrodes in lithium-ion cells Carbon. 50: 5359-5371. DOI: 10.1016/J.Carbon.2012.07.009  0.643
2011 Bhattacharya S, Riahi AR, Alpas AT. Role of voltage scan rate on degradation of graphite electrodes electrochemically cycled vs. Li/Li+ Materials Research Society Symposium Proceedings. 1388: 20-25. DOI: 10.1557/Opl.2012.8  0.736
2011 Bhattacharya S, Riahi AR, Alpas AT. In-situ observations of lithiati on/de-lithiation induced graphite damage during electrochemical cycling Scripta Materialia. 64: 165-168. DOI: 10.1016/J.Scriptamat.2010.09.035  0.74
2011 Bhattacharya S, Riahi AR, Alpas AT. A transmission electron microscopy study of crack formation and propagation in electrochemically cycled graphite electrode in lithium-ion cells Journal of Power Sources. 196: 8719-8727. DOI: 10.1016/J.Jpowsour.2011.05.079  0.739
2009 Bhattacharya S, Riahi AR, Alpas AT. Indentation-induced subsurface damage in silicon particles of Al-Si alloys Materials Science and Engineering A. 527: 387-396. DOI: 10.1016/J.Msea.2009.08.052  0.718
Show low-probability matches.